How should waterproof case seals be maintained?
Clean the channel before the lid comes down, inspect the gasket for a hard flattened set once a season, close every latch so the rim is loaded evenly instead of tightening one corner, and store the case open or with the latches released. That is the whole routine, and it is worth more than any product you could add to it. A sealed case keeps water out at exactly one place - the line where the lid rim meets the base rim with a compressible gasket between them - and almost every field leak is that line being held open by grit, by a gasket that has lost its recovery, or by a lid that flexes between widely spaced latches. On our published catalogue 124 of 155 model listings record a compressible gasket in a continuous moulded channel and 31 record that no seal is offered on that shell, so the routine is written per model, not per range; and we publish no water-ingress result for any of the 155, because a maintenance page and a performance claim are different documents.
Key points
- Most field leaks are a contaminated channel or a set gasket, not defective rubber: clean and inspect the rim before you judge anything else.
- Store a sealed case open, or with the latches released. A gasket left compressed inside a closed shell for months loses the recovery that seals it.
- Never over-latch a leaking corner. Excess compression accelerates the set that opened the gap; the answer is a new gasket or a flatness check.
- Sealing is published per model, not per series: 124 of our 155 listings record a gasket in a continuous moulded channel and 31 record none offered.
- Every model that publishes a gasket channel also publishes a wall of 3.0 mm or more, median 4.2 mm; unsealed bodies sit at 2.9 mm or thinner.
- Latch count is recorded as specified per configuration, so on a wide flat lid you have to order the corner compression rather than inherit it.
- A pressure-equalisation valve is offered on all 155 models and fitted as standard on none: it manages air pressure, and it is one more path to inspect.
- Water, dust, ultraviolet, service temperature, stack load, load capacity and any protection rating are recorded as unmeasured on all 155 models.
What waterproof case seals maintained actually asks of you
The phrase a buyer types is waterproof case seals maintained, and what sits behind it is a routine rather than a product. Four checks and one habit cover almost everything. Check one: before the lid comes down, the channel and the gasket are wiped or flushed clear of grit, sand and dried salt. Check two: once a season the gasket is run through by hand for a hard, shiny, flattened section - the permanent set that means the strip can no longer bridge the two moulded faces. Check three: every latch is closed, so the rim is loaded across the whole footprint instead of at the two points that happen to have hardware. Check four: the join and any cut length are looked at, because that is where a gasket lifts first. The habit is the storage state: a sealed case that lives shut with its latches cranked is a case that ages its gasket twice as fast as one stored open.
None of that requires a laboratory. It matters because the sealing line is a mechanical joint with a small margin. A compressible gasket is asked to deform into the microscopic waviness of two moulded surfaces and stay there while the shell flexes, expands in heat and contracts in cold. The waviness is measured in tens of microns; an angular grain of beach sand is a hundred times that. This is why a case that leaked at month fourteen usually has nothing wrong with its rubber and everything wrong with the state of its rim on the morning it was closed, and why a maintenance page is worth more to a fleet than a specification sentence.
What the seal on our cases is, in the words of our own data
Two fields in our published product data describe the sealing, and they carry different weight. The construction is recorded as measured: the model page states whether the shell carries a compressible gasket seated in a continuous moulded channel, and 124 of the 155 listings say yes while 31 state that no seal is offered on that shell. A channel moulded as part of the body is the point - it holds the gasket at a fixed position and thickness all the way round, where a glued strip relies on its adhesive at exactly the corners where the lid moves most. The compound is recorded as a manufacturer option: EPDM or equivalent compressible gasket, which means the elastomer you receive is a line on your order, agreed per configuration, not a fixed property of a catalogue line.
The channel is also the thing that collects. Sand from a beach, grit from a vehicle bed, dried salt from spray, trim tailings from a moulding floor, lint from a rag - all of it settles in a groove that is doing its job by being compressed. So the order of operations in any leak investigation is fixed: clean first, then look at the rubber, then look at the hardware, and only after those three look honest does it make sense to talk about the shell. A supplier who starts at the fourth step is selling you a replacement case.
The five ways a maintained seal still fails
Maintenance is aimed at named failure modes, not at a general sense of care. These are the five that produce the enquiries we actually receive, with what you can see at the case and what our published data does and does not say about each one.
| How The Sealing Line Fails | What You See At The Case | What To Do | What Our Data Publishes |
|---|---|---|---|
| Contamination in the channel | The lid closes but one corner sits proud; a damp line on the foam after rain | Flush with fresh water, dry the groove, close on a clean rim and re-check the gap by eye | Channel continuity per model on 124 of 155 listings; no water result on any model |
| Compression set in the gasket | A hard, shiny, flattened band, usually along one long edge or under the latches | Replace the gasket; do not tighten the latches to compensate for lost recovery | Gasket recorded as measured construction, compound recorded as an order option |
| Lid flex between widely spaced latches | The middle of the longest edge is wet while the corners are dry | Specify the latch count for that footprint at quotation stage, and check wall thickness | Latch count as specified per configuration; wall thickness on 148 of 155 models |
| A distorted rim or a damaged parting line | A gap you can feel with a fingernail, or a lid that no longer sits flush | Retire or repair the shell; flatness cannot be maintained back into a distorted rim | Nothing - geometry is published as nominal figures, not as a flatness result |
| A penetration added after delivery | Moisture appears near a drilled cable port, an added hasp or a fitted gland | Treat the modified case as a new assembly with no history and re-plan the closure | Pressure-equalisation valve as an option on all 155 models, fitted as standard on none |
Cleaning the rim: what to use, and what to keep off it
Fresh water and a soft brush do most of the job. After sea spray or a wet sandy day, flush the channel rather than wiping a dry rim: a cloth dragged across a salted groove pushes crystals back into it, and salt is hygroscopic, so the residue it leaves keeps drawing moisture against the gasket long after the case looked clean. Then let the channel dry before the lid comes down. Closing a wet rim traps water against the elastomer and against the foam below it, and a damp interior is a different problem from an ingress problem - it is the one that corrodes a instrument's own connectors and grows mould on a fabric strap.
What to keep off the gasket is a longer list than buyers expect. Solvent wipes, degreasers, petroleum-based cleaners and abrasive pads all attack an elastomer that is being asked to recover. On the shell side our published materials are polypropylene on 94 models, engineering polypropylene on 38, ABS on 22 and one PP/ABS combination, and the two families behave differently around a cleaning regime: polypropylene tolerates fuels, lubricants and cleaning agents that field equipment travels with better than ABS does, while ABS gives a stiffer panel and a better printing face. That is a material argument, not a test record. If your site insists on a chemical cleaner, ask for the cleaner's own technical sheet and check it against the gasket compound you ordered, and never paint a sealing rim - paint in a channel holds the gasket off its seating permanently.
Inspecting the gasket: set, nicks and the join
Do it by hand and do it the whole length. Run a thumb along the strip and feel for a section that has gone hard, glossy or visibly thinner - that is compression set, and it is not repairable. A quick field test is a fingernail press into the face of the strip: a healthy compressible gasket springs back, a set one leaves a dent. Check the join or the cut length especially closely, because that is where a strip lifts first and where a lifted join looks like a leaky shell. Then check for nicks and abrasion along the run where the lid met the base most often, and for any section that has been squashed by something caught in the rim - a cable, a strap, a corner of a hard case packed on top of it.
Treat the gasket as a service item in the same category as a tyre or a filter. We publish the construction of the seal as measured data and the compound as an option; we do not publish a service interval, because the honest answer depends on your storage state, your cleaning regime, your temperature swing and your lot. The replacement itself is straightforward on our shells, since the seal is a standard compressible profile seated in a moulded channel rather than a one-off extrusion tied to a single order - which is exactly the serviceability question a buyer should ask a supplier before committing to a fleet: can the gasket be replaced from a stocked part, and can the channel be cleaned with a brush and fresh water?
Latch compression, lid stiffness and the mid-span gap
A gasket cannot compensate for a lid that moves. Compression in the middle of the longest edge is what fails, because the two corners nearest the latches are held and the span between them is not. That is why the sealing construction and the structural data have to be read together on the same model page. On our catalogue every model that publishes a gasket channel also publishes a wall thickness of 3.0 mm or more, with a median of 4.2 mm, while the unsealed bodies that publish a wall sit at 2.9 mm or thinner with a median of 2.2 mm. That is not a performance claim of any kind. It is the plain consequence of a factory selling thin shallow shells unsealed, because a compressible strip in a supported channel on a lid that flexes between two latches leaks however good the rubber is.
The lid-to-base split decides where the stiffness lives. The split is published on 100 models, with lid depth from 16 mm to 320 mm and base depth from 15 mm to 168 mm, a median of 44 mm at the base. Take four sealed shells from the published sheets: KX-1905 carries a 3.0 mm wall with a 25 mm lid over a 15 mm base, a compact body whose short spans mean little mid-span flex; KX-4616 is a 3.0 mm wall with an even 74 mm lid over 74 mm base; KX-5321 puts almost all its depth in the base, 43 mm of lid over 149 mm on a 5.8 mm wall; and KX-88442 is the opposite shape again, a 320 mm lid over a 44 mm base on a 5.0 mm wall with two wheels, which is the geometry where the middle of a long lid edge most needs the latch count to be specified rather than assumed.
| Model | Internal Mm | Wall Mm | Lid Over Base Mm | Net G | Why It Is Here |
|---|---|---|---|---|---|
| KX-1905 | 180 x 160 x 40 | 3.0 | 25 over 15 | 250 | Short spans; mid-span flex is small by geometry |
| KX-4010 | 390 x 315 x 88 | 3.0 | 44 over 44 | 1015 | Wide flat lid, narrow width 282 mm inside a 315 mm nominal width |
| KX-4616 | 455 x 338 x 148 | 3.0 | 74 over 74 | 1395 | Even split; either half can carry the sealing load |
| KX-65522 | 507 x 385 x 190 | 5.3 | not published | 4860 | ABS shell, three units to a 565 x 450 x 665 mm carton |
| KX-5321 | 481 x 373 x 192 | 5.8 | 43 over 149 | 4810 | Deep base keeps mass away from the lid wall and its rim |
| KX-97227 | 590 x 435 x 210 | 6.0 | 42 over 168 | 10000 | Thickest published wall, on wheels and published non-stackable |
Over-packing: the leak that starts inside the case
The second most common cause of a case that will not seal is not dirt, it is contents. Usable interior volume is published against nominal volume on every one of our 155 models and is smaller than nominal on 154 of them, with the ratio running from 0.797 to 1.000 and a median of 0.850, because radiused corners, wall thickness and hardware all take space that a drawing rectangle does not show. A layout planned from nominal figures leaves the lid looking shut while the sealing line is being held fractionally open by the load beneath it.
The taper figure makes the same problem less obvious. A narrow internal width is published on 36 models, from 70 mm to 308 mm: on KX-4010 the nominal internal width is 315 mm but the narrow width is 282 mm, so a rigid item can clear the sidewall at the front and press against it near the parting line, where that pressure ends up on the rim. Check the fit by closing the empty case with the packed load inside and looking at the gap all the way round before you accept a delivery, and specify the interior from a drawing, a photograph of the packed kit or a physical sample rather than from a general description of the contents.
Storage, cartons and the year that quietly kills a gasket
Compression set happens while a case is idle, not while it is being carried. Our packing data makes that concrete for the buying decision: carton dimensions are published on 64 models and pieces per carton on 58, running from 1 to 40 per carton with a median of 10, which means a sealed case normally ships and is stored closed, inside a carton, with its gasket already under load from the day it was packed. If a sealed model is going to sit in a depot for a year before issue, decide the storage state at order time and write it into the packing instruction, because a compressed year in a hot store is a plausible way to receive a fleet that needs new gaskets before it needs equipment.
Then there is breathing. A case carried from an air-conditioned room into hot humid weather, or left in the sun and then rained on, has internal air that expands and contracts through the rim; the joint is being pumped, and what gets drawn in with each cycle is whatever is floating around it. A pressure-equalisation valve exists to relieve that cycle, and it is recorded as a configuration option on all 155 models and fitted as standard on none. Two things follow. First, a valve manages air pressure, not water, so it is not a waterproofing device and it does not substitute for rim maintenance. Second, choosing to fit one adds a penetrator to the closure, which is one more item to inspect and one more reason a later modification is a new assembly. Where cases are stacked, note also that 136 models are published stackable and all 19 wheeled models are published non-stackable, because the wheel housings and the handle channel occupy the rim and base area a column would otherwise bear on.
If a seal has already failed, in what order to act
Work through it as a short decision tree. Clean and dry the channel, then close on an empty cavity: if the gap closes evenly, the previous leak was contamination or contents, and the fix is the routine plus a packing change. If the gap is still open along one edge, look for a set band in the gasket in the same place; replace the strip. If a new strip in the same shell still shows a gap, the rim or the lid flatness is the problem, and the shell should be retired or assessed rather than cranked shut with extra latch force. If moisture keeps appearing near a hole that was drilled after delivery, no closure work will help, because the water is coming in somewhere else and the assembly you are maintaining is not the assembly that was built.
What you cannot do is compare your case against a catalogue number, because there is no number to compare it with. Water, dust, ultraviolet, service temperature, stack load, load capacity and any protection rating are recorded as unmeasured on all 155 of our models, and no ingress code is stated for any of them. Where your own programme genuinely needs a documented result - a tender, a warranty exposure, an audit - the route is to freeze the configuration, then commission accredited testing of that model with that gasket compound, that latch count, that valve decision and that interior as a separate work package, and receive the report for the article that was tested. We will tell you plainly which figures we hold as production data, which we can build but have not tested, and which need a laboratory.
What a stated protection class means, and what to ask any supplier for
Buyers often arrive with a class or a standard name in their specification, so it is worth being clear about what such a name is. A two-digit ingress code, for example, is a pair of laboratory results: the first digit records a solid-particle duty and the second records a water duty, each with its own apparatus, its own duration and its own pass criterion. It is not a ladder on which a bigger number means a better box in every respect, and it is not a property of the plastic or of the rubber - it is a statement about one closed assembly put through one procedure. That is why the code alone, without the method behind it, is nearly useless in an audit: the same digits can be produced by quite different exposures, and a result taken on an empty shell says nothing about the same shell loaded with a radio and a cable gland added later.
So the honest questions to put to any supplier are procedural rather than numerical. Which method was used and to which revision. What apparatus. What the specimen was - model, wall, gasket compound and lot, latch count, valve fitted or blanked, interior as shipped. What the exposure actually was: depth and duration, or flow and standoff, and at what temperature differential. How many articles, and what happened to any that failed. What counted as ingress: indicator tape, a weighed pad, a visual check, a functional test of the contents. Who ran it and whether that body holds accreditation for the method. And who holds the report, because a document you cannot cite has little value in your own compliance file.
The same structure applies to military specification standard numbers, to a stated drop height, to repeated handling shock, to flammable-atmosphere equipment categories, to airdrop qualification and to electrostatic discharge behaviour: each is a separate procedure with its own specimen rules, and none of them is answered by an adjective. Our own position is deliberately narrow. We do not print a class in a catalogue or inherit a result from a neighbouring size, because we do not hold those records; we publish the construction we can verify on the part; and where a customer tender requires a named result we say whether it exists and, if it does not, we quote accredited testing on the exact configuration you are ordering as its own work package. If a supplier tells you a case is simply rated, ask for the report first - it takes a minute and it settles the argument.
Choosing a sealed case you can actually keep working
Write the exposure before you look at a product. A case stored indoors and carried to a vehicle, one left in an open boat locker, one hosed at a wash-down point and one dropped in and recovered are four different duties, and only the last two push you towards commissioning a test. Then size the cavity from published internal dimensions on the packed load, never from the external row: on KX-65522 the body measures 545 by 440 by 215 mm outside and 507 by 385 by 190 mm inside, so a plan built from the external figure loses the walls, the rim and the hardware, and a load that loses the rim is a leak you will blame on the gasket.
After that, the four things that decide how maintainable the seal is. One: whether the model is one of the 124 listings that publish a gasket in a continuous moulded channel or one of the 31 sold unsealed. Two: the published wall thickness and lid-to-base split, because rim stiffness between the latches is what protects the sealing line. Three: latch count as an ordered configuration rather than an inherited default, especially on a wide flat lid. Four: serviceability - a stocked gasket profile, a channel a brush can reach, a case that can be stored open, and a document pocket or valve decision made at order rather than drilled later. A specification that fails the fourth item will need new gaskets inside a year whatever it was built with.
Where the routine earns its keep
The duties that justify a maintained seal share one feature: the case is opened somewhere other than where it was stored. Coastal and marine communications, survey and hydrographic instruments, field medical kits that live in a vehicle bay overnight, environmental and agricultural measurement programmes, optics and camera loads, and the telecommunications case a service engineer leaves on wet grass for a working day. Across our published catalogue 148 of 155 models carry the outdoor application tag, 140 carry electronics and all 155 carry field-equipment, which is where these enquiries usually land.
In those roles the enemy is usually condensation and repeated entry rather than a wave: the case cools at night, draws humid air in as the lid cracks open, and the moisture condenses on a cold board or a cold lens. A clean, recovering gasket slows that process; a wipe-before-closing habit and a dry storage state are what stop it. The reverse case is equally worth stating: a shell that only ever travels indoors is buying a maintenance obligation it does not need, and an unsealed body from the same series is often the better engineering choice and always the cheaper one to keep.
Customising the closure under an OEM order
Sealing geometry is set by the mould and is not tuned per order, so the useful decisions sit around it. The interior is the cheapest: a cut layout in pick-and-pluck, die-cut or CNC-cut form, in PE, EVA or EPE, is produced from a drawing, a photograph of the packed kit or a physical sample, and custom foam starts at a single set, which is how a fit that does not lift the rim gets proven before a fleet is committed. Colour, printed logo and identification, and OEM production on an existing moulding, start at 300 pieces, with a first sample planned at 45 days on a 30 per cent deposit and the balance paid after your inspection. A pressure valve, a document holder and a padlockable latch arrangement are configuration lines on the same order - the latch body on our shells accepts a standard padlock, which is recorded as measured across all 155 models.
A genuinely new exterior geometry is a mould project: about 125 days and from 3,000 pieces per moulded component, because changing the wall, the rib pattern or the channel changes the sealing you would later be maintaining. Anything added by others after delivery - a gland, a feed-through, a cut-out for a display, a bolt-on hasp - converts the assembly into a different assembly, so tell us at quotation stage where a pass-through is unavoidable and the gasket route and the hardware can be designed around it instead of through it.
Procurement notes and the four questions to ask in writing
Ask four things of any supplier, in writing, and most seal disputes disappear before an order is placed. Which models are published with a gasket in a continuous channel and which are not. Is the gasket replaceable from a stocked profile, and what is the part reference for the model you are buying. How many latches compress the rim on the size you are ordering, and can the count and positions be changed. And is any performance figure you have been given traceable to a report naming that model and that configuration. Then check the completeness of the sheet rather than its tone: in our own data net weight is published on 93 of 155 models, wall thickness on 148, the lid-to-base split on 100, pieces per carton on 58, and gross weight on none, so a supplier whose tables are uniformly full is a supplier to question, not to admire.
KeXin New Materials (Guangdong) Co., Ltd. manufactures for wholesale and OEM buyers only, quoted EXW or FOB from the factory, with no retail channel, no delivered-duty-paid arrangement and no overseas warehouse stock, so inbound freight is planned by your own forwarder against the factory term. Third-party inspection of finished goods and of the factory is welcome at any time. Send the packed dimensions and mass of the load, the exposure you are maintaining against, the quantity per delivery and the destination, and we return candidate models with their published sealing construction, internal and usable volume, wall thickness, lid-to-base split, net weight where recorded and carton data, together with a gasket and latch plan you can put on a maintenance sheet. Fred Zhao, KeXin Sales Team, WhatsApp +86 135 3588 0002.




Customisation
Everything described above is configurable on a standard shell: interior layout (pick-and-pluck, die-cut or CNC-cut), foam grade and thickness, colour, logo method, latch and lock count, pressure-equalisation valve, cable ports, document holder and identification plate. A bespoke exterior geometry requires a new mould — 125 days, from 3,000 units per moulded component.
Procurement considerations
| Question | What to send us |
|---|---|
| Which shell fits? | Equipment L × W × H as packed, plus required clearance per axis |
| What does it cost? | Order quantity and estimated annual quantity — the two drive different answers |
| Is tooling needed? | Whether an existing shell clears the envelope with usable foam depth |
| Lead time? | Your required delivery date, not just the order date |
| Certification? | The exact standard your tender names — we will say whether we can test to it |
| Freight? | Destination and preferred terms; carton and pallet data supplied with the quotation |
Comparison and selection guide
The tables on this page exist because a protective case is chosen by comparing three things: the envelope, the environment and the handling chain. Where no table applies, the rule below is.
| Situation | What To Do |
|---|---|
| Occasional splash | A close-fitting rim without a gasket is cheaper and easier to maintain. |
| Rain and washdown | Sealed configuration, four or more latches, stainless hardware. |
| Immersion or pressure change | Sealed configuration plus a pressure-equalisation valve, and a documented test. |
- Size on internal dimensions plus clearance, never on a product name.
- Choose the carrying method before the shell: it changes the series, not just the price.
- Specify the interior last, and decide up front whether the end user will reconfigure it.
How should waterproof case seals be maintained? relates to Waterproof & Dustproof Guide. Related families: Waterproof Cases / Outdoor Protective Cases / Military Protective Cases / Instrument & Equipment Cases / Electronics Cases / Communication Equipment Cases / Camera & Photography Cases / Custom Protective Cases. Related sectors: field and industrial equipment. Continue in the Waterproof & Dustproof Guide cluster.
This page is written from our own production data. If your requirement differs, send the dimensions and we will tell you which of the 155 models fits, or whether a custom route is needed.